Steinberg - Lund

type name
steinberg-lund
parameters
rho0			reference density
g0 ya			initial shear modulus, athermal flow stress
a b			pressure and temperature dependence of shear modulus
beta n eps0 ystarmax	work hardening
gamma0 amelt tm0	melt
t0			reference temperature (usually 300 K)
c1 c2 Tact yp		rate-dependence
ytmin			minimum yt, e.g. 1.0e-8